Old 05-28-2015, 09:37 AM   #2
Bill Baer
Senior Member
 
Join Date: Jul 2007
Location: Nothern IL
Posts: 596
Likes: 1
Liked 1 Time in 1 Post
Default Re: Mild steel cage material.

DOM is DRAWN OVER MANDREL so there is no seam line inside of the tubing. EWS is just standard mild steel tubing the only advantage of the DOM is the more exact Inner diameter. DOM is more expensive than EWS.
I Personally would give S&W call and ask them.
Since your roll cage will be ultra sonic thickness tested, I would consider going up one wall thickness size from the minimum required.
Tubing as manufactured has a tolerance .120 wall tubing may be .118-.122 an it can get even thinner on the outside of a bend.
While slightly thicker tubing is a little heavyer it can be a huge PITA to change out a tube in a completed roll cage.
__________________
Bill Baer 3391 SC, 339B SC, QR
Bill Baer is offline   Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 07:19 PM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.
Copyright Class Racer.com. All Rights Reserved. Designated trademarks and brands are the property of their respective owners.