Dave's method is similar to mine, although I use red hi temp RTV. The suggestion to use the metal core cork gasket is a good one as well.
On the timing cover I always use a gasket, and install it dry first to set my cam end play, and then use a super thin layer of the same red hi temp RTV for final assembly.